HI folks, iv just got my first Printer, went with the flash force Creator Pro, got it setup and working and am playing today with the small Marvin figurine from 3d hubs,

I am after some set advice, initial print was poor, iv reduce speed and its better but its got sagging around the, front, ears and lower back ares, also i can see distinct colour diferance between the top half and bottom half of the model, goes from dark at the bottom to lighter at the top with the big shift in the middle.

thanks

===

[IMG]http://img.photobucket.com/albums/v202/hundleton1/Firstline/10F2DB11-D779-4514-9E94-535C89AA5339\_zpsqneihmo4.jpg\[/IMG\]

[IMG]http://img.photobucket.com/albums/v202/hundleton1/Firstline/8113807B-AC7B-4610-8CDE-38A7EDF9DE89\_zpsberadtp9.jpg\[/IMG\]

[IMG]http://img.photobucket.com/albums/v202/hundleton1/Firstline/EF925C93-FA06-4F58-8A0F-A5B19A8055BA\_zpscrza5uys.jpg\[/IMG\]

[IMG]http://img.photobucket.com/albums/v202/hundleton1/Screen%20Shot%202015-10-23%20at%2016.37.51\_zpsedeydlpc.png\[/IMG\]

Hi

Are you using PLA?

Yea boy much better results with 190 extruder, 50 bed and speed down to 40mms

Hope you are using external cooling when printing with PLA. PLA does not require a heated bed but cooling is essential.

hi yea initially was pla, mostly got that sorted now apart from larger prints are delaminating,

now onto abs

will post pictures shortly

I have problem with Marvin print too.

I tried 40-60 mm/s

210-350 temp

85-110 bed

But top keyring twisted and bootom warped and burned. At 235C white abs will be lite brown.